Prevent corrosion, contamination and blockages
Text Lieke BousemaImage KOREX Benelux

The most common problems and solutions in water treatment for closed systems
In recent years, the number of WKO systems in the Netherlands has risen sharply. This is hardly surprising, since, combined with low-temperature heat emitters such as underfloor heating, underfloor cooling and low-temperature radiators, these systems can ensure a comfortable indoor climate in every season, with minimal energy consumption. One condition is that the system water is treated correctly, from commissioning through to the end of the system’s service life. If this is not done, or is done inadequately, the following problems, among others, may arise, according to Mario van Gorsel, director of KOREX Benelux:
Construction debris and sludge
“Unfortunately, many installers still underestimate how much construction debris and sludge ends up in, for example, the connecting and riser pipes of closed systems during construction. This includes dust, sand, welding particles, welding flux and microfibres, which settle on the bottom along with the lime particles released, preventing the system from passivating itself,” says Van Gorsel. “In this case, the pH of the heating water is constantly being neutralised. The system will therefore remain corrosive, resulting in significant losses in efficiency and comfort, as well as faults and failures in valves, shut-off valves, controllers, pumps and other components.”
To remove construction debris and sludge from the system, it must first be flushed. “The dirt can then be removed from the system by filtration. The DEEL-SEP bag filter with stainless steel housing can help with this.” It is important to mobilise the contamination. “For example, adding an inhibitor (corrosion inhibitor/protective agent) prevents the dirt from settling. A second, measured dose of liquid can then be used to bring the pH up to the desired level, step by step.” The system must be degassed to control this process properly and prevent the pH from being neutralised.

Contamination and blockages
The introduction of low-temperature systems has reduced water volumes and pipe diameters. “The latter in particular regularly causes problems, because blockages occur more readily,” says Van Gorsel. “To prevent this, contamination must be captured promptly and effectively.” When large quantities of fine magnetic particles settle in the system, rooms do not heat up sufficiently. “Systems can also develop faults, and consumption-based billing is no longer reliable. To address this problem, the protective layer in the system must be restored. Mobilising the contamination, filtration and degassing are essential here too.”
Incorrect and/or excessive use of inhibitors
When an inhibitor (corrosion inhibitor/protective agent) is used, it must be applied correctly and in exactly the right quantity to keep the conductivity and alkalinity of the system water low, says Van Gorsel. “In practice, however, so much is often added that the conductivity of the system water becomes too high and, combined with low hardness, galvanic corrosion occurs.” Corrosion of materials such as steel and aluminium is only possible if the water is electrically conductive, he emphasises. An inhibitor is not needed for this. “If too much or the wrong inhibitor is used, it is advisable to flush the system completely and start the water treatment process again.”

Incorrect combinations of materials
Van Gorsel also notes that different materials are still used too often in systems. One example is a combination of copper and stainless steel, which can lead to galvanic corrosion. “In galvanic corrosion, the less noble material (the anode) is generally attacked, while the more noble material (the cathode) is protected against corrosion,” he explains. “The anode material will corrode, leading to pitting and eventually significant leaks. One way to prevent this, commonly used in the shipping industry, is to install a sacrificial anode. This solution is also suitable for closed systems, where a magnesium oxide anode should preferably be added and inspected and replaced periodically.”
For anyone wishing to find out more about keeping the water quality in closed systems in optimum condition, VDI 2035-1, Sheet 2, is an excellent guide. It provides a detailed description of the requirements from design and commissioning through to the full period of use, maintenance and any modifications.
When passivating the heating water in a closed system, it is important to follow these steps:
- Fill the system with tap water (pH-neutral).
- Heat the system water to reduce the oxygen content (thermal degassing).
- The residual oxygen will react chemically with the corrosion present in the system and then dissolve in the water.
- As the oxygen content falls further, the pH will rise. Once the pH exceeds 8.2, the corrosion pressure in the system is negligible.
A business enquiry for KOREX Benelux? Get in touch
Companies in this story